Surface hardness of different restorative materials after long-term immersion in sports and energy drinks
Ugur ERDEMIREsra YILDIZMeltem Mert ERENSevda OZEL
Author information
JOURNAL FREE ACCESS

2012 Volume 31 Issue 5 Pages 729-736

Details
Abstract

The purpose of this study was to evaluate the effect of sports and energy drinks on the surface hardness of different restorative materials over a 6-month period. Forty-two disk-shaped specimens were prepared for each of the four restorative materials tested: Compoglass F, Filtek Z250, Filtek Supreme, and Premise. Specimens were immersed for 2 min daily, up to 6 months, in six storage solutions (n=7 per material for each solution): distilled water, Powerade, Gatorade, X-IR, Burn, and Red Bull. Surface hardness was measured at baseline, after 1 week, 1 month, and 6 months. Data were analyzed statistically using repeated measures ANOVA followed by the Bonferroni test for multiple comparisons (α=0.05). Surface hardness of the restorative materials was significantly affected by both immersion solution and immersion period (p<0.001). All tested solutions induced significant reduction in surface hardness of the restorative materials over a 6-month immersion period.

Content from these authors
© 2012 The Japanese Society for Dental Materials and Devices
Previous article Next article
feedback
Top