Color changes of dental zirconia immersed in food and beverage containing water-soluble/lipid-soluble pigments
Hiro MATSUMOTOTakatsugu YAMAMOTOTohru HAYAKAWA
Author information
JOURNAL FREE ACCESS Advance online publication

Article ID: 2022-021

Details
Abstract

The present study examined color changes in the tooth-colored restorative materials, zirconia (3Y-TZP), resin composite, and porcelain. The colors (CIELab) of these materials were measured using a spectrophotometer. Specimens were immersed in black tea or curry for 1 and 7 days, after which colors were re-assessed. Color differences (∆E*ab) before and after immersion were calculated. Specimens after the 7-day immersion were ultrasonically cleaned, and colors were measured again to assess the color recovery rate. The surface free energy, roughness, and water sorption/solubility of each material were also evaluated. Specimens were observed under a scanning electron microscope. The ∆E*ab of 3Y-TZP was the smallest with both immersions. Resin composite had the smallest recovery rate. The surface free energy and roughness of 3Y-TZP were smaller than those of porcelain. 3Y-TZP and porcelain showed almost no sorption during the 7-day period. The present results revealed that 3Y-TZP exhibited the strongest resistance to discoloration.

Content from these authors
© 2022 The Japanese Society for Dental Materials and Devices
feedback
Top