  • Naoyuki MISHIMA, Soichi KURIYAMA, Hirokazu SHIBAGAKI, Masao YOSHINARI, ...
    Type: Original
    2017 Volume 30 Issue 2 Pages 86-93
    Published: June 30, 2017
    Released: August 05, 2017
    JOURNALS FREE ACCESS

    Ultraviolet (UV) treatment of titanium produces a hydrophilic surface on the titanium and enhances osteoblast attachment, proliferation and differentiation. It is reported that differences in storage conditions influence the sustainability of hydrophilicity of titanium surfaces after ultraviolet treatment. However, there are no reports regarding the relationship between the change of hydrophilicity of titanium surfaces during storage and biological properties. In the present study, the influence of time-dependent changes of hydrophilicity of ultraviolet treated titanium on protein adsorption was investigated. As protein, fibronectin, which is a cell adhesive protein, was used. Titanium was stored in a desiccator under atmospheric conditions for 1 day, 3 days, 1 week, 2 weeks and 1 month after ultraviolet treatment. As a control, a titanium surface immediately after UV treatment (0-day) was employed.
    First, contact angles against water at different storage periods were measured. Fibronectin adsorption behavior was monitored by the quartz crystal microbalance (QCM) method. Amounts of fibronectin adsorbed onto the titanium sensor and apparent adsorption rate were obtained using QCM measurements.
    The contact angle after 1-day storage was almost seven times higher than that of the 0-day titanium surface (p<0.05). The contact angle gradually increased with the storage period. After 1-week storage, the degree of increase of contact angle became smaller.
    A significantly large degree of frequency decrease by fibronectin adsorption was observed at 0-day by QCM measurement (p<0.05). Longer storage periods of UV treated titanium resulted in a smaller degree of frequency decrease. Calculation of adsorption amounts of fibronectin by the frequency decrease curve revealed that the adsorbed amount at only 1-day storage was significantly less than that at 0-day (p<0.05). The adsorbed amounts of fibronectin to 1-day or 3-day stored titanium were significantly greater than that to 1-month stored titanium (p<0.05). The apparent adsorption rate was obtained by curve fitting of the frequency decrease curve. The apparent adsorption rate of 1-day and 3-day storage significantly reduced to less than half of that of 0-day storage (p<0.05).
    In conclusion, atmospheric storage of UV treated titanium changed the hydrophilic titanium surface to a hydrophobic surface and significantly reduced the adsorption amounts and apparent adsorption rates of fibronectin to titanium even for only 1-day storage.

    Download PDF (1035K)
  • Kiyoshi AKIMOTO, Yasunori KOUNO, Toshiro HIDAKA, Naoki IMAMURA, Satosh ...
    Type: Original
    2017 Volume 30 Issue 2 Pages 94-101
    Published: June 30, 2017
    Released: August 05, 2017
    JOURNALS FREE ACCESS

    This study examined the effects of changing the sampling sites of Ti-6Al-4V alloy manufactured by the wire drawing method on the hardness, elastic modulus, fatigue fracture, corrosion resistance, and observed structure of the alloy. The following results were obtained.
    It was clarified that the hardness, elastic modulus, fatigue fracture, corrosion resistance, and structure of Ti-6Al-4V alloy manufactured by the wire drawing method were influenced by the sampling site. The test pieces parallel with the drawing direction were significantly inferior to those perpendicular to the drawing direction. It was thought that the extended α-phase in the drawing direction had an influence on this phenomenon. The material used to produce biomaterials should have uniformly excellent corrosion resistance and mechanical properties at all positions of the material.

    Download PDF (1551K)
Survay and Statistics
  • Kazushige ISOBE, Yuji KOKUBO, Mitsuyoshi TSUMITA, Kazuhisa OKADA, Chik ...
    Type: Survay and Statistics
    2017 Volume 30 Issue 2 Pages 102-110
    Published: June 30, 2017
    Released: August 05, 2017
    JOURNALS FREE ACCESS

    The aim of this clinical study was to evaluate the technical complications of implant-supported single crowns at Tsurumi University Hospital. The patients who received implant-supported single crowns from January 2004 to April 2014 received follow-up examinations and evaluations of technical complications. The patients attended at least once a year, and all crowns functioned for more than 1 year. A total of 536 implant-supported single crowns were examined with regard to the location, type of implant, type of connection, and time of failure event. The results were as follows : 1. Technical complications were observed in 15% of crowns after placement ; 2. Screw loosening was the most frequent complication, followed by fracture or chipping of facing material ; 3. 75% of screw loosening occurred within 1 year after placement ; 4. Most fractures or chippings of facing materials were observed in screw-retained crowns placed in the molar region.

    Download PDF (813K)